Fig. 4: Accuracy of DeepThin under a variety of conditions. | npj Computational Materials

Fig. 4: Accuracy of DeepThin under a variety of conditions.

From: Quantifying defects in thin films using machine vision

Fig. 4: Accuracy of DeepThin under a variety of conditions.

In the top row, the accuracy for reproducing the human-labeled scores for the extent of cracking and the extent of dewetting in an image is shown. In all other rows, the accuracy for correctly classifying the images based on the presence or absence of different morphological defects is shown. Empty cells in the figure are associated with defects that were not present in the datasets or were not labeled for this study. Images in each row have the same scale. Scale bars from top to bottom are 500 µm, 50 µm, 50 µm, and 12.5 µm.