Fig. 10: TEM images of the passive films of the samples at the OCP in 3.5 wt. % NaCl solution for 3600 s.
From: Corrosion behavior of TiZrHfBeCu(Ni) high-entropy bulk metallic glasses in 3.5 wt. % NaCl

a TC sample. b, c EDS mapping images of the test area corresponding to a. d TN sample. e, f EDS mapping images of the test area corresponding to d.