Table 3 The results of SCC sensitivity factor.
From: Improvement of stress corrosion cracking resistance by low cycle fatigue of a CrNiMoV steel
Fatigue cycles | Ib (%) | Is (%) | Iφ (%) | It (%) | IA (%) |
|---|---|---|---|---|---|
0 | 2.67 | 1.92 | 85.36 | 88.45 | 56.67 |
5000 | 4.57 | 4.76 | 78.53 | 89.59 | 50.40 |
10,000 | 6.41 | 6.86 | 73.81 | 90.02 | 51.36 |
15,000 | 7.65 | 6.45 | 73.40 | 87.71 | 51.91 |
20,000 | 3.35 | 2.54 | 72.94 | 87.64 | 49.35 |