Fig. 7: Variation in quantified degradation indicators along the cross section of the coatings.

MSFL is shown in the left column and the intensity of the 1780 cm−1 band is shown as a function of distance to surface for the pigmented systems. Both columns show averages and standard deviations of the values found within an ~17 µm wide area of the drilled hole.