Fig. 3: CrCoNi metal ion release after 28 d of corrosion.
From: Long-term corrosion studies of CrCoNi and CrMnFeCoNi in sulfuric acid

Fraction of dissolved metal ions of CrCoNi after 28 d of immersion, as determined by ICP-MS with their average concentrations.