Table 5 Percentage of every damage mechanism for 30 min wear of samples in simulated seawater

From: Enhancing mechanical strength and tribological performance in tin bronze alloys via rolling treatment

Samples

Mass loss caused by different interaction components (mg)

Mt

Mf

Mc

Mcf

Mfc

wire-arc DED

2.96

2.58

4.84×10−3

6.24×10−2

0.31

rolled alloy

2.23

1.93

6.87×10−3

3.0×10−2

0.26