Table 7 Wire-arc DED parameters in the experiment

From: Enhancing mechanical strength and tribological performance in tin bronze alloys via rolling treatment

parameters

Current (A)

Frequency (Hz)

Swing (mm)

Voltage (V)

Speed (cm·min−1)

Line-energy (J·cm−1)

Energy density (J·cm−2)

Value

65

10

24

0.6

4

84.6

1523.4