Table 1 Initial and final compositions of the viscosity measurement samples.

From: Estimation of TiO2-FeO-Na2O slag viscosity through molecular dynamics simulations for an energy efficient ilmenite smelting process

(mol%)

Initial composition

Final composition

FetO

TiO2

Na2O

FeO

Fe2O3

TiO2

Na2O

Fe2+/(total Fe)

FT46

40.0

60.0

 

31.9

3.0

65.1

 

0.91

FT55

50.0

50.0

 

46.6

2.7

50.7

 

0.95

FT64

60.0

40.0

 

54.1

3.0

42.9

 

0.95

FT46N3

38.8

58.2

3.0

32.7

2.4

62.2

2.7

0.93

FT46N6

37.6

56.4

6.0

24.6

6.4

63.8

5.2

0.79

FT46N9

36.4

54.6

9.0

23.6

6.8

60.1

9.4

0.78