Table 1 Porous structure parameters of UIO, ACPMG, UIO/ACPMG10% nanohybrid, UIO/ACPMG20% nanohybrid and UIO/ACPMG30% nanohybrid.

From: Enhanced VOCs adsorption with UIO-66–porous carbon nanohybrid from mesquite grain: A combined experimental and computational study

Material

SBET (m2/g)

Vt (cm3/g)

Pore volumeBJH

Average pore diameter (nm)

UIO

1505

0.780

0.240

2.120

ACPMG

1428

1.060

0.640

2.990

UIO/ACPMG10%

866.470

0.530

0.244

2.454

UIO/ACPMG20%

980.420

0.560

0.246

2.280

UIO/ACPMG30%

878.860

0.550

0.274

2.50

UIO/ACPMG20% after adsorption

672.270

0.470

0.211

0.223