Table 4 SC Interface parameters as fed in the simulation.
From: Salutary impact of spontaneous oxidation in CH3NH3SnI3 on CZTS-based solar cell
Sr. no. | Parameters | CH3NH3SnI3/CZTS (HTL/Absorber) | CZTS/CdS (Absorber/ETL) |
|---|---|---|---|
1. | Defect | neutral | neutral |
2. | Concentration (\({cm}^{2}\)) | \({10}^{10}\) | \({10}^{10}\) |
3. | Energy w.r.t reference (eV) | 0.600 | 0.600 |
4. | Energetic distribution | single | single |
5. | Capture cross section electrons (cm²) | \({10}^{-19}\) | \({10}^{-19}\) |
6. | Capture cross section holes (cm²) | \({10}^{-19}\) | \({10}^{-19}\) |
7. | Reference for defect energy level Et | Above the highest EV | Above the highest EV |