Table 4 Parameters a and B in Eq. (1) obtained from fitting experimental data.

From: Synthesis of long-chain polyester polymers and their properties as crude oil pour point depressant

Solution

A

B

R2

DW

-8138.83

30.738

0.99981

DW + 2% PVP

-8215.16

31.019

0.99939

DW + 2%PVP + 0.1% P-PPD

-8295.12

31.321

0.99957

DW + 5% EG

-9028.83

34.126

0.99986

DW + 2%PVP + 5% EG

-8840.04

33.467

0.99823

DW + 2%PVP + 5% EG + 0.1% P-PPD

-9037.3

34.167

0.99826