Table 2 Investigated DEM parameters with their low, middle and high values (\(\:{\mu\:}_{s}=\) coefficient of sliding friction, \(\:{\mu\:}_{r}=\) coefficient of rolling friction, \(\:{C}_{r}=\) coefficient of restitution). The underlined values for pellet-pellet and sinter-sinter parameters used for pellet-sinter interactions.
Factor | Low level (-1) | Middle level (0) | High level (+ 1) | |
|---|---|---|---|---|
Pellet-pellet | \(\:{\mu\:}_{s,pp}\) | 0.2139 | 0.455 | 0.740 |
\(\:{\mu\:}_{r,pp}\) | 0.0541 | 0.145 | 0.2438 | |
\(\:{C}_{r,pp}\) | 0.342 | 0.5 | 0.743 | |
Sinter-sinter | \(\:{\mu\:}_{s,\text{s}\text{s}}\) | 0.4344 | 0.595 | 0.7638 |
\(\:{\mu\:}_{r,\text{s}\text{s}}\) | 0.0835 | 0.23 | 0.3838 | |
\(\:{C}_{r,\text{s}\text{s}}\) | 0.0145 | 0.18 | 0.3538 | |
Pellet-sinter | \(\:{\mu\:}_{s,\text{p}\text{s}}\) | 0.21 | 0.485 | 0.76 |
\(\:{\mu\:}_{r,ps}\) | 0.05 | 0.215 | 0.38 | |
\(\:{C}_{r,ps}\) | 0.01 | 0.355 | 0.7 | |
Pellet-geometry | \(\:{\mu\:}_{s,pg}\) | 0.3142 | 0.405 | 0.546 |
\(\:{\mu\:}_{r,pg}\) | 0.0542 | 0.2 | 0.3540 | |
\(\:{C}_{r,pg}\) | 0.243 | 0.41 | 0.6238 | |
Sinter-geometry | \(\:{\mu\:}_{s,\text{s}g}\) | 0.3834 | 0.64 | 0.947 |
\(\:{\mu\:}_{r,\text{s}g}\) | 0.0835 | 0.14 | 0.234 | |
\(\:{C}_{r,\text{s}g}\) | 0.0547 | 0.275 | 0.545 |