Table 3 The apparent rate constants and half life times for photocatalytic degradation of acid red 37 dye using UV/TiO2, UV/SnO2, UV/TiO2–SnO2 (97:3), UV/TiO2–SnO2 (90:10) and UV/TiO2–SnO2 (80:20).
Catalytic system | Catalyst loading (g/L) | kapp (min−1) | t1/2 (min) |
|---|---|---|---|
UV/TiO2 | 0.4 | 2 × 10−4 | 346.0 |
UV/SnO2 | 0.4 | 28 × 10−4 | 247.1 |
UV/TiO2–SnO2 (97:3) | 0.4 | 38 × 10−4 | 182.1 |
UV/TiO2–SnO2 (90:10) | 0.4 | 72 × 10−4 | 96.1 |
UV/TiO2–SnO2 (80:20) | 0.4 | 35 × 10−4 | 197.7 |