Table 3 Mixing scheme of mortars.

From: Experimental studies on mix design and properties of ceramic-glass geopolymer mortars using response surface methodology

Mix

Binder (mass%)

NH: NS

S: B

Oven duration (hr)

Curing times (days)

CWP

RGP

PC

C90N2S0.7

90

10

–

2

0.7

12, 24

3, 28

C90N0.5S0.7

90

10

–

0.5

0.7

12, 24

3, 28

C90N2S0.5

90

10

–

2

0.5

12, 24

3, 28

C80N1S0.5

80

20

–

1

0.5

12, 24

3, 28

C100N2S0.6

100

–

–

2

0.6

12, 24

3, 28

C80N1S0.7

80

20

–

1

0.7

0, 6, 9, 12, 24

3, 28

C100N1S0.7

100

–

–

1

0.7

12, 24

3, 28

C90N1S0.6

90

10

–

1

0.6

12, 24

3, 28

C80N2S0.6

80

20

–

2

0.6

12, 24

3, 28

C100N1S0.5

100

–

–

1

0.5

12, 24

3, 28

C90N0.5S0.5

90

10

–

0.5

0.5

12, 24

3, 28

C80N0.5S0.6

80

20

–

0.5

0.6

0, 6, 9, 12, 24

3, 28

C100N0.5S0.6

100

–

–

0.5

0.6

12, 24

3, 28

Control sample

–

–

100

–

0.6*

0

3, 28

  1. *For PC control sample, S: B refers to water: solid ratio