Fig. 16
From: Nanoscale 3D spatial analysis of FTO/ZnO/Ag-x films subjected to photocatalytic activity

Nyquist plots of Ag/ZnO films (a) under both dark and illuminated conditions using NaOH electrolyte solution and (b) the circuit model corresponding to energy diagram FTO/ZnO/Ag@electrolyte interface.