Table 1 Specifications of prepared samples.
From: Nanoscale 3D spatial analysis of FTO/ZnO/Ag-x films subjected to photocatalytic activity
Sample no. | Sample name | Compounds | Doping ratio |
|---|---|---|---|
1 | FTO/ZnO/Ag-0 | 0.6 M zinc acetate dehydrate ~ 6.5847 g | 0% Ag |
2 | FTO/ZnO/Ag-2 | 0.6 M zinc acetate dihydrate ~ 6.5847 g 0.3 M silver nitrate ~ 0.2938 g | 2% Ag |
3 | FTO/ZnO/Ag-4 | 0.6 M zinc acetate dihydrate ~ 6.5847 g 0.3 M silver nitrate ~ 0.5999 g | 4% Ag |
4 | FTO/ZnO/Ag-6 | 0.6 M zinc acetate dihydrate ~ 6.5847 g 0.3 M silver nitrate ~ 0.9190 g | 6% Ag |
5 | FTO/ZnO/Ag-8 | 0.6 M zinc acetate dihydrate ~ 6.5847 g 0.3 M silver nitrate ~ 1.2520 g | 8% Ag |