Fig. 8

(a–d) Afterglow decay curves of Sr1.94MgSi2O7: Eu2 + 0.01, Dy3 + 0.05 phosphors with different silicium-strontium ratios and (e) dependence of the initial brightness of the afterglow on sintering temperature.

(a–d) Afterglow decay curves of Sr1.94MgSi2O7: Eu2 + 0.01, Dy3 + 0.05 phosphors with different silicium-strontium ratios and (e) dependence of the initial brightness of the afterglow on sintering temperature.