Table 2 XRF analysis of WRMB and KDP.

From: Treatment of recycled concrete aggregate with magnesium phosphate cement

Sr. No

Chemical Composition (%)

MgO

Al2O3

SiO2

Ca0

Fe2O3

SO3

K2O

Cr2O3

Cl

P2O5

ZrO2

1

WRMB

75.435

8.423

8.231

3.237

2.485

0.808

0.276

0.266

0.175

0.171

0.160

2

KDP

–

–

–

–

0.02

0.80

41.08

 

0.2

57.84

–

Sr. No

Chemical Composition (%)

TiO2

MnO

V2O5

CuO

Zn0

NiO

As2O3

SrO

Ir2O3

Rb2O

 

1

WRMB

0.118

0.101

0.049

0.023

0.014

0.012

0.009

0.006

0.002

–

 

2

KDP

–

0.01

–

–

0.01

–

–

–

–

0.01

Â