Table 2 Peak current (Ip) and Electrochemically Active Surface Area (EASA) of plasma-printed ZnO and CeO2 electrodes at different plasma voltages.
From: Direct printing of metal oxide nanostructures for wearable electrochemical sensing
Sample Name | Printing Voltage (kV) | Peak Current Ip (µA) | Electrochemically Active Surface Area (cm²) |
|---|---|---|---|
Bare SPE | 0 | 30.103 | 0.0256 |
ZnO_16kV | 16 | 52.843 | 0.045 |
ZnO_18kV | 18 | 54.981 | 0.0468 |
ZnO_20kV | 20 | 56.210 | 0.0479 |
CeO2_22kV | 22 | 329.692 | 0.281 |
CeO2_24kV | 24 | 420.945 | 0.359 |
CeO2_26kV | 26 | 434.07 | 0.370 |