Table 6 Comparison of the properties of this work with other reported studies.
Parameter | Current work | ||||
|---|---|---|---|---|---|
Additives (ppm) | 100MgO, 100La₂O3, 300ZrO2 | 500 MgO | 100MgO− 100La2O3 | 450 MgO− 450Y2O3− 450ZrO2 | 100MgO, 400Y2O3 |
Fracture toughness (MPa.m1/2) | 5.24 | 4.8 | 5.1 | 4.9 | – |
Flexural strength (MPa) | 356 | 320 | 340 | 310 | 193 |
Visible light transmission (700 nm, %) | 32 | 28 | 30 | 25 | 13 |
Infrared transmission (5 µm, %) | 71.4 | 61 | 67 | 68 | 60 |
Synthesis method | (SPS) | (SPS) | (SPS) | (SPS) | (SPS) |