Table 1 An exposition of the dataset employed in the present study.
| Â | Mean | STD | Min | Max |
|---|---|---|---|---|
Input parameters | ||||
 Compressive strength (CS)—Mpa | 30.82 |  ± 8.71 | 20 | 51 |
 Minimum cover (Cmin)—mm | 51.78 |  ± 23.35 | 19 | 112.5 |
 Diameter of steel Bar (db)—mm | 14.84 |  ± 4.15 | 8 | 25 |
 Bond length (Ld)—mm | 113.97 |  ± 92.81 | 39 | 500 |
 Corrosion level (Cw)—% | 6.25 |  ± 6.44 | 0 | 29 |
 Yield strength of steel bar (YS)—MPa | 472.59 |  ± 82.25 | 258.68 | 600.3 |
Output parameters | ||||
Ultimate bond strength (UBS)—Mpa | 8.58 |  ± 6.61 | 0.19 | 27.80 |
Relative bond strength (RBS) | 0.71 |  ± 0.35 | 0.01 | 1.57 |