Table 4 Mechanical properties of the as-received alloys.
Run | conditions | UTS | YS | El% | HV |
|---|---|---|---|---|---|
AR 1050 AA | As received alloy | 70.6 | 32.79 | 30 | 29 |
AR 2011 AA | As received alloy | 235 | 130 | 16 | 90 |
AR 6063 AA | As received alloy | 89.6 | 43.3 | 28 | 44 |
Run | conditions | UTS | YS | El% | HV |
|---|---|---|---|---|---|
AR 1050 AA | As received alloy | 70.6 | 32.79 | 30 | 29 |
AR 2011 AA | As received alloy | 235 | 130 | 16 | 90 |
AR 6063 AA | As received alloy | 89.6 | 43.3 | 28 | 44 |