Table 3 Differences in the mechanical properties of marble under different confining pressure conditions.

From: Experimental and numerical investigation on mechanical properties and fracture mechanisms of deep marble under triaxial compression

Confining pressure

Fracture characteristics

Post-peak deformation capacity

Peak stress

Cohesion

Friction angle

Low confining pressure(<30 MPa)

Brittle failure

Insignificant

Significantly improve

Relatively low

Relatively high

High confining pressure(≥30 MPa)

Ductile failure

Significant

The increase is not significant

Relatively high

Relatively low