Table 6 Comparison of the room temperature maximum ionic conductivity of different solid biopolymer electrolytes.
Host matrix | Dopant salt | Ionic conductivity\(\:\:\left(\text{S}\:{\text{c}\text{m}}^{-1}\right)\) | Ref. |
|---|---|---|---|
CS | NH4I | \(\:3.73\times\:{10}^{-7}\) | |
CS: Corn Starch | NH4Cl | \(\:6.47\times\:{10}^{-7}\) | |
CS | NaTF | \(\:7.34\times\:{10}^{-7}\) | |
CS | NH4CF3SO3 | \(\:1.00\times\:{10}^{-6}\) | |
CS: PVA | NH4I | \(\:1.77\times\:{10}^{-6}\) | |
CS: PS | KSCN | \(\:2.32\times\:{10}^{-6}\) | |
FSG | LiClO4 | \(\:3.58\times\:{10}^{-6}\) | |
CS: MC | LiBF4 | \(\:3.74\times\:{10}^{-6}\) | |
CS: PS | NH4SCN | \(\:1.07\times\:{10}^{-5}\) | |
FSG | NH4NO3 | \(\:1.52\times\:{10}^{-5}\) | |
CS: Dx | MgCl2 | \(\:1.79\times\:{10}^{-5}\) | |
CS: FSG | NH4SCN | \(\:1.19\times\:{10}^{-5}\) | This work |