Table 1 The effect of reaction parameters with actual and predicted values for MG degradation.

From: Hydrolyzed MOF based Mo@h-ZIF-8/ZnS composite for enhanced photodegradation of dye pollutants using a combined experimental and RSM approach

Run

H2O2 dosage (A) (mM)

Catalyst dosage (B) (mg)

Dye concentration (C) (ppm)

Time (D) (min)

Degradation efficiency (%)

Residual

Experimental

Predicted

1

0.08

4

60

40

90.13

90.76

− 0.6304

2

0.08

8

60

40

92.14

92.28

− 0.1396

3

0.06

6

70

50

98.9

98.90

0.0000

4

0.06

6

90

50

93.8

93.08

0.7200

5

0.06

2

70

50

91.3

90.20

1.10

6

0.04

4

60

60

91.54

92.03

− 0.4854

7

0.06

6

50

50

94.47

94.09

0.3767

8

0.06

6

70

50

98.9

98.90

0.0000

9

0.04

8

60

60

93.4

93.88

− 0.4796

10

0.04

4

80

40

87.31

87.88

− 0.5688

11

0.06

6

70

50

98.9

98.90

0.0000

12

0.08

8

80

60

94.7

94.84

− 0.1379

13

0.1

6

70

50

93.3

92.78

0.5183

14

0.08

4

60

60

95.16

95.21

− 0.0479

15

0.06

6

70

50

98.9

98.90

0.0000

16

0.08

4

80

60

93.16

94.13

− 0.9688

17

0.04

8

60

40

90.06

89.74

0.3229

18

0.02

6

70

50

88.67

88.09

0.5783

19

0.06

6

70

50

98.9

98.90

0.0000

20

0.06

6

70

50

98.9

98.90

0.0000

21

0.06

6

70

30

88.4

88.02

0.3833

22

0.04

4

80

60

91.67

91.98

− 0.3113

23

0.04

8

80

60

93.45

93.47

− 0.0154

24

0.08

8

60

60

96.21

96.29

− 0.0771

25

0.08

4

80

40

90.19

90.16

0.0287

26

0.06

10

70

50

93.2

93.20

− 0.0033

27

0.06

6

70

70

96.84

96.13

0.7133

28

0.04

4

60

40

87.13

87.44

− 0.3129

29

0.04

8

80

40

89.4

89.80

− 0.4029

30

0.08

8

80

40

91.15

91.31

− 0.1604