Table 2 Refractive index and thickness of au/cqds thin film exposed to different concentrations of UA ranging from 0 µM to 1.0 µM.
UA concentration (µM) | CQDs layer | ||
|---|---|---|---|
Refractive index | Thickness (nm) | ||
n | k | ||
0 | 1.343 | 0.1137 | 12.00 |
0.05 | 1.344 | 0.1087 | 12.00 |
0.1 | 1.350 | 0.1037 | 12.00 |
0.5 | 1.355 | 0.0907 | 12.00 |
1.0 | 1.372 | 0.0827 | 12.20 |