Table 2 Particle size distribution data, RMS, AR of KLa2-xSrxCoO4 films prepared at different Sr doping.
\(\:{\mathbf{L}\mathbf{a}}_{2-\mathbf{x}}{\mathbf{s}\mathbf{r}}_{\mathbf{x}}\mathbf{C}\mathbf{o}{\mathbf{O}}_{4}\) | Thickness (nm) | Mean size (nm) | FWHM (nm) | AR | RMS(nm) |
|---|---|---|---|---|---|
0.5 | 537 | 37.66 | 13.7 | 2.74 | 6.80 |
0.7 | 519 | 43.47 | 12.6 | 3.45 | 11.23 |
0.9 | 551 | 55.07 | 14.36 | 3.83 | 15.67 |
1.1 | 546 | 41.41 | 13.6 | 3.04 | 7.49 |
1.3 | 519 | 53.67 | 14.26 | 3.76 | 12.21 |