Fig. 10

Compressive strength of tuff tiles produced with varying proportions (5%, 10%, 15%) of different agricultural and industrial byproducts, demonstrating that sugarcane bagasse ash at 5% replacement achieved the highest strength (~ 32 MPa).

Compressive strength of tuff tiles produced with varying proportions (5%, 10%, 15%) of different agricultural and industrial byproducts, demonstrating that sugarcane bagasse ash at 5% replacement achieved the highest strength (~ 32 MPa).