Table 3 Physio-mechanical properties of Ceiba Pentandra fiber.

From: Evaluation of nonfired ceramic tiles using phosphogypsum waste and Ceiba Pentandra fiber for sustainable construction

Property

Value

Fiber diameter (mm)

0.42

Density (g/cm3)

1.19

Poison’s ratio

0.21

Tensile strength (GPa)

2.74

Young’s modulus (GPa)

59.1

% of elongation

1.46