Table 2 Parameters of DMA creep TTS testing.
From: Applying high-performance resins in stereolitography printing to produce prototype injection moulds
Parameters used | Unit | Typical value |
|---|---|---|
Bending stress | MPa | 5 |
Minimum temperature | °C | 30 |
Maximum temperature | °C | 170 |
Temperature increment between 30 °C and 95 °C | °C | 5 |
Temperature increment between 95 °C and 170 °C | °C | 25 |
Furnace time | min | 10 |
Creep time | min | 30 |
Recovery | min | 30 |
Atmosphere | Air | |