Fig. 6

h0l layer of Fe0.975Cu0.025Te0.66Se0.34 crystal measured at room temperature at 3.5, 7.2, and 10.7 kbar, respectively (from left to right). All data presented in the above panel were obtained for the same crystal (with the same orientation matrix) enclosed in a modified Merrill–Bassett Diamond-Anvil Cell.