Table 2 Thickness of oxide layer after oxidation at 1450 °C for 5 h for all samples.

From: Synergetic and alone influence of graphite platelet and SiC on the oxidation resistance of ZrB2 ceramics

Sample

Zr

Zr10GP

Zr15GP

Zr15Si

Zr30Si

Zr30Si10GP

Zr30Si15GP

Thickness, µm

129 ± 5

112 ± 5

80 ± 4

62 ± 5

38 ± 3

40 ± 4

64 ± 5