Fig. 3
From: Deep eutectic solvents and mango peel extract as active ingredients of Pva films

Thermogravimetric analysis results for the PVA-based films: (
) for the temperature at which a 5% mass loss is observed T5%, (
) for a 10% mass loss T10% and (
) for a 50% mass loss T50%.