Table 3 The contrast between tempering and hardening.

From: Geometric influence and multi-objective optimization of WEDM for hardened tool steels using ANN and NSGA-II

Performance measures

Hardening

Tempering

Temperature range

980–1020 °C

600–610 °C

Time

12 min

20 min

Achieved HRC

62

40