Table 3 EDX results: Ratio normalised to Ni as 8, to compare with input 8:1:1 ratio.

From: Laser diagnostic investigation on flame-assisted spray synthesis of NMC811 battery materials

 

Before calcination

After calcination

Ni

Co

Mn

Ni

Co

Mn

ratio

8

1.04

0.93

8

1.06

0.99