Fig. 9

SEM microstructure of bimetallic composite Sp. 9 sintered at 1300 °C: (a) Overview of WC-Co/LCS interface; (b) Enlarged view of region II; (c) Enlarged view of region I; (d) Enlarged with mag. at 4000×view of region III.

SEM microstructure of bimetallic composite Sp. 9 sintered at 1300 °C: (a) Overview of WC-Co/LCS interface; (b) Enlarged view of region II; (c) Enlarged view of region I; (d) Enlarged with mag. at 4000×view of region III.