Table 2 Partitioning coefficient of selected alloying elements in the alloy 718 + TiB2 nanocomposites processed by suction casting.

From: Microstructure, phase transformation temperatures and long-term stability of ex-situ Alloy 718 + TiB2 metal-ceramic nanocomposites as a repair coatings for aerospace applications

Addition of TiB2 to Alloy 718, %

Ni

Cr

Fe

Mo

Nb

Ti

Al

0

1.01 (± 0.03)

0.99 (± 0.01)

1.08 (± 0.02)

1.31 (± 0.07)

0.41 (± 0.09)

0.99 (± 0.22)

1.22 (± 0.44)

1.25

1.02 (± 0.03)

1.03 (± 0.01)

1.11 (± 0.01)

1.00 (± 0.18)

0.47 (± 0.03)

0.46 (± 0.08)

0.93 (± 0.29)

2.5

1.04 (± 0.02)

1.00 (± 0.01)

1.10 (± 0.01)

0.95 (± 0.11)

0.44 (± 0.06)

0.51 (± 0.12)

0.98 (± 0.21)

3.75

0.98 (± 0.02)

1.10 (± 0.01)

1.09 (± 0.01)

1.50 (± 0.16)

0.56 (± 0.04)

0.51 (± 0.16)

1.03 (± 0.39)

5.0

0.94 (± 0.02)

1.16 (± 0.05)

1.08 (± 0.02)

2.80 (± 0.25)

0.57 (± 0.05)

0.54 (± 0.08)

1.54 (± 0.13)