Table 1 Mix proportion of laterite improved with geopolymer and MNRL.

From: Toughness enhancement of geopolymer stabilized laterites using para rubber latex for sustainable base and subbase applications

Symbol

FA content

(%)

MNRL content

(%)

Symbol

FA content

(%)

MNRL content

(%)

F20N0

20

0

F30N0

30

0

F20N5

5

F30N5

 

5

F20N7

7

F30N7

 

7

F20N10

10

F30N10

 

10

F25N0

25

0

F35N0

35

0

F25N5

5

F35N5

 

5

F25N7

7

F35N7

 

7

F25N0

10

F35N10

 

10