Table 3 Composition of HPDC mixture (kg/m3).

From: Rebar free high performance ductile concrete beams powered by CFRP and post-tensioning

Cement

SF

GGBFS

Silica sand

w/b ratio

Micro steel fiber (volume fraction)

580

131

588

652

0.19

2.0%