Table 4 Specifications and proportions of the tested mixtures.

From: Mechanical behavior and microstructural investigation of loess sustainable stabilization using nanosilica and GGBS

 

Mixture

FTCs

Curing time (day)

UCS

CP

UPV

BET

FTIR

XRD

SEM

1

Loess

Loess

0, 1, 4, 10

1

2

 + 0.4% NS

3

 + 0.7% NS

4

 + 1% NS

5

 + 1.3% NS

6

 + 1% NS

5% GGBS

0, 1, 4, 10

7 and 28

28

7

10% GGBS

8

15% GGBS

9

20% GGBS