Table 6 Flexural strength (MPa).

From: Study on the mechanics and self-sensing properties of ultrahigh-performance shotcrete containing waste glass aggregates

 

0%GS

25%GS

50%GS

75%GS

100%GS

0%SF

6.42

6.56

6.13

6.51

6.67

0.5%SF

12.25

12.14

11.82

12.00

12.37

1.0%SF

14.76

15.16

14.84

14.52

15.00

1.5%SF

18.62

18.93

19.28

19.73

19.59

2.0%SF

21.38

20.74

21.28

22.03

21.69