Fig. 2
From: Lithium recovery from mixed spent LFP-NMC batteries through atmospheric water leaching

Recovery of lithium from NMC black mass at varying of (a) heating rate (950 °C, 2 h) and (b) temperature (15 °C/min, 2 h).
From: Lithium recovery from mixed spent LFP-NMC batteries through atmospheric water leaching

Recovery of lithium from NMC black mass at varying of (a) heating rate (950 °C, 2 h) and (b) temperature (15 °C/min, 2 h).