Table 2 Tensile procedures of the SLM316LSS XOY samples during in situ neutron diffraction.
Number | Control by force (N) | Control by displacement (mm) |
|---|---|---|
1 | 0 | |
2 | 1650 | |
3 | 3300 | |
4 | 4950 | |
5 | 6600 | |
6 | 8250 | |
7 | 9075 | |
8 | 9900 | |
9 | 2 | |
10 | 2.5 | |
11 | 3 | |
12 | 3.5 | |
13 | 4 | |
14 | 5 | |
15 | 6 | |
16 | 7 | |
17 | 7.5 | |
18 | 8 | |
19 | 8.5 | |
20 | 9 | |
21 | 9.5 | |
22 | 10 | |
23 | 11 | |
24 | 13 | |
25 | 13.6 |