Table 9 Loss in weight of all mixtures after exposure to MgSO4 solution.

From: Durability and environmental evaluation of rice husk ash sustainable concrete containing carbon nanotubes

Mix. No.

Weight loss (%)

No. of cycles

1

2

3

R15C0

0.15

0.221

0.269

R15C10

0.062

0.07

0.103

R15C15

0.069

0.098

0.113

R15C20

0.115

0.124

0.132