Table 2 Textile coating procedure.
(PET) | (PAD 6,6) |
|---|---|
1. Treatment of 20 × 20 cm samples in two liters of 0.02 M/l Mg (NO3)2.6H2O solution for 30 min. | 1. Treatment of 20 × 20 cm samples in two liters of 0.02 M/l Mg (NO3)2.6H2O solution for 30 min. |
2. Hydrolytic formation of Mg (OH)2 by gradual addition of 0.04 M/l NaOH solution for 30 min. | 2. Hydrolytic formation of Mg (OH)2 by gradual addition of 0.04 M/l NaOH solution for 1 h. |
3. Rinsing and centrifugation. | 3. Rinsing and centrifugation. |
4. Thermal stabilization in a thermopress at 150 °C for 30 min. | 4. Thermal stabilization in a thermopress at 140 °C for 30 min. |