Table 3 Mix proportions of LSP mortar.
From: Laterite soil powder as cementing material for the production of high-performance mortar
Mix code | Binders | W/C ratio | Water (ml) | Sand (g) | Superplasticizer (ml) | |
|---|---|---|---|---|---|---|
OPC (g) | LSP (g) | |||||
LSA 0% | 820 | – | 0.32 | 250 | 984 | 14.06 |
LSA 10% | 738 | 82 | 0.32 | 250 | 984 | 14.06 |
LSA 20% | 656 | 164 | 0.32 | 250 | 984 | 14.06 |
LSA 25% | 615 | 205 | 0.32 | 250 | 984 | 14.06 |