Table 1 Chemical composition of copper slag powder and cement (%).
From: The LS/CS ratio-performance relationship in DG-activated hybrid cements
Material | CaO | Al2O3 | SiO2 | Fe2O3 | MgO | K2O | P2O5 | SO3 | LOI* |
|---|---|---|---|---|---|---|---|---|---|
CS | 1.68 | 8.64 | 30.91 | 50.38 | 0.60 | 1.54 | 0.07 | 0.47 | 5.71 |
LS | 25.4 | 20.7 | 33.5 | 3.10 | 0.70 | 5.20 | 0.20 | 7.50 | 3.70 |
C | 61.29 | 5.03 | 20.56 | 3.88 | 1.79 | 1.56 | 0.15 | 2.59 | 3.15 |