Table 2 Raw material ratio (wt%) of prepared samples.

From: The LS/CS ratio-performance relationship in DG-activated hybrid cements

Sample

C

CS

LS

DG*

W/C

C0

100

0

0

0

0.4

1-CLS

70

0

30

6

0.4

2-CSC

70

30

0

6

0.4

3-CCL

70

20

10

6

0.4

4-CCL

70

15

15

6

0.4

5-CCL

70

10

20

6

0.4

  1. *Remark: The DG dosage calculated as an external addition (extra 6% by weight of the total binder).