Table 1 Comparison of our work with similar structures of spintronic devices, highlighting the enhanced MR in ultraclean 2D materials-based spintronic devices
From: Unpinning the magnetic interface between 2D materials and NiFe for ultra-low coercivity spin valves
Structure | MR(%) | Temperature | Method | Reference |
|---|---|---|---|---|
Co/Gr/Co | 0.7 | 1.5 K | Exfoliation | |
Co/Gr/Co | 1.0 | 1.5 K | Exfoliation | |
Co/Gr/NiFe | 0.23 | 10 K | Wet transfer | |
Co/Gr/NiFe | 0.1 | 10 K | Similar to UCD | |
NiFe/Gr/NiFe | 0.4 | 77 K | Exfoliation | |
NiFe/Gr/NiFe | 0.14 | 10 K | Wet transfer | |
NiFe/Gr/NiFe/NiO(pinned-SV) | 2.3 | 10 K | UCD | Our work |
NiFe/Gr/NiFe(pristine-SV) | 1.3 | 10 K | UCD | Our work |