Fig. 2
From: Understanding charge compensation mechanisms in Na0.56Mg0.04Ni0.19Mn0.70O2

In situ XRD patterns of Na0.56Mg0.04Ni0.19Mn0.70O2 galvanostatically cycled. Cells have been cycled using electrolyte of 1 M NaPF6 in PC at a rate of 15 mA/g. Measured XRD patter during a the first cycle, b the second cycle and c the third cycle